X6NiCrTiMoVB25-15-2, 1.4980, 1.3980, 1.4606, 1.4944, A-286, Grade 660 steel - Special heat-resistant austenitic chromium-nickel steel with carbide-forming elements according to PN-EN 10302, PN-EN 10088-1 and PN-EN 10269.

 

Standards Steel Grades
Chemical Composition %
C: Mn: Si: P: S: Cr: Mo: Ni: V: Ti: Al: B: Ce:
EN / DIN X6NiCrTiMoVB25-15-2 - X 6 NiCrTiMoVB 25-15-2 - 1.4980 - 4980
0.03 - 0.08 1.0 - 2.0 <1.00 <0.025 <0.015 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.30 <0.35 0.003 - 0.010 -
SEW 390 X5NiCrTiMoV26-15 - X 5 NiCrTiMoV 26-15 - 1.3980
<0.8 <2.0 <1.0 <0.030 <0.015 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.9 - 2.3 <0.35 0.003 - 0.010 -
EN X5NiCrTiMoVB25-15-2 - 1.4606
<0.08 1.0 - 2.0 <1.00 <0.025 <0.015 13.0 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.30 <0.35 0.001 - 0.010 -
AFNOR Z5NCTDV25-15B - Z 5 NCTDV 25-15 B - XN26AW - X.N26A.W
<0.05 <2.00 <0.75 <0.030 <0.015 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.80 - 2.30 <0.40 0.0025- 0.008 -
GOST 08Ch15N25T2MFR - EP674 - EP 674 - 08Kh15N25T2MFR - 08Х15Н25Т2МФР - ЭП674
<0.08 1.2 - 1.7 <0.70 <0.020 <0.015 14.0 - 16.0 1.1 - 1.6 24.0 - 26.0 0.2 - 0.4 1.90 - 2.40 <0.30 <0.0100 <0.01
AFNOR Z6NCTDV15-15B - Z 6 NCTDV 15-15 B - X.N26T.W - XN26TW - X.N 26 T.W
0.03 - 0.08 <2.00 <1.00 <0.020 <0.015 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.30 <0.35 0.0025 - 0.008 -
LW X4NiCrTi25-15 - 1.4944 - LW 4944
<0.08 <2.00 <1.00 <0.025 <0.015 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.30 <0.35 0.003 - 0.010 -
UNS S66286 - S 66286 - K66286 - K 66286
<0.08 <2.00 <1.00 <0.040 <0.030 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.35 <0.35 0.001 - 0.010 -
RA A-286 - A 286 - Alloy 286 - Grade 660
<0.08 <2.00 <1.00 <0.040 <0.030 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.35 <0.35 0.001 - 0.010 -
GB/T 06Cr15Ni25Ti2MoAlVB
<0.08 <2.00 <0.04 <0.040 <0.030 13.5 - 16.0 1.0 - 1.5 24.0 - 27.0 0.1 - 0.5 1.90 - 2.35 <0.35 0.001 - 0.010 -

 

Steel 1.4980, A-286, Grade 660 - Specification

Heat resistant steel with high strength, creep resistance, low magnetic permeability and high oxidation resistance. Endurance properties are obtained by emitting MC, M6C carbides by means of nickel, titanium and aluminum.

It retains the appropriate mechanical properties to a temperature of about 650 - 700 ℃. In addition, it exhibits suitable strength properties at extremely low temperatures. Heat resistant to a temperature of about 800 - 900 ℃.

Used as a steel for aviation and power engineering for heavy-duty rotors, gas turbine blades, steam turbines, pressure equipment parts and reactors, jet engines and rockets, exhaust systems. Also used in cryogenics and cryotechnics.


Mechanical properties of steel - X6NiCrTiMoVB25-15-2, 1.4980

Mechanical properties
Tensile strength Rm 900 - 1150 MPa
Yield point Re > 600 MPa
Elongation A > 15%
Density ρ 8.00 kg/dm3
Modulus of elasticity E 211 GPa
Coefficient of thermal expansion α 17.0 - 18.5 ⋅ 10-6 K-1
Heat conductivity λ20℃ 13 W ⋅ m-1 ⋅ K-1

 


Mechanical properties at different temperatures X6NiCrTiMoVB25-15-2, 1.4980

Mechanical properties at temperatures
Properties Temperatures
50℃ 100℃ 150℃ 200℃ 250℃ 300℃ 350℃ 400℃ 450℃ 500℃ 550℃ 600℃ 650℃ 700℃ 750℃
Yield point Re (MPa) >592 >580 >570 >560 >550 >530 >520 >510 >500 >490 >460 >430 >380 >295 >200

 


List of equivalents and other determinations of X6NiCrTiMoVB25-15-2, 1.4980 steel:

X 6 NiCrTiMoVB 25-15-2, 4980, X5NiCrTiMoVB25-15-2, 1.4606, Z5NCTDV25-15B, Z 5 NCTDV 25-15 B, XN26AW, X.N26A.W, 08Ch15N25T2MFR, EP674, EP 674, 08Х15Н25Т2МФР, ЭП674, Z6NCTDV15-15B, Z 6 NCTDV 15-15 B, X.N26T.W, XN26TW, X.N 26 T.W, X4NiCrTi25-15, 1.4944, LW 4944, S66286, S 66286, K66286, K 66286, A-286, A 286, Alloy 286, 06Cr15Ni25Ti2MoAlVB, EZ6NCT25, FE-PA2601, FE-PA92-HT, Grade 660.