Stainless ferritic steel X2CrNi12, 1.4003, AISI 410L with the addition of Nickel and Nitrogen according to EN 10088-1.

 

Standard Steel Grade
Chemical Composition %
C: Mn: Si: P: S: Cr: Ni: N:
EN X2CrNi12 - X 2 CrNi 12 - 1.4003
<0.03 <1.5 <1.0 <0.04 <0.030 10.5 - 12.5 0.3 - 1.0 <0.03
ASTM UNS S40977
<0.03 <1.5 <1.0 <0.04 <0.015 10.5 - 12.5 0.3 - 1.0 <0.03
JIS G4303 - SUS 410L - SUS 410 L
<0.03 <1.0 <1.0 <0.04 <0.030 11.0 - 13.5 <0.6 -

 

Specifications and application

X2CrNi12 is a stainless steel with ferritic structure, which chemical composition from 0H13, X6Cr13, 1.4006, AISI 410S deviates from the original by a small addition of Nickel, and even more limited content of Carbon. Chromium at a concentration of approx. 12% allows users to use the material as a building material in non-aggressive environments, including decorative purpose.

 

Steel does not show resistance to acids, chlorides, salts or marine environments to such an advanced extent as austenitic steels. For applications as a corrosion-resistant material, coating of the material and proper surface treatment is required. The products can be used to produce components and decorative elements in the construction industry, or parts of vehicles in the communication and automotive industries.

 

Steel also found in the food, mining and sugar industries. .In addition, X2CrNi12 is easily weldable, has relatively good mechanical properties in annealed condition +A, at room and elevated temperatures.


Mechanical properties of X2CrNi12, 1.4003 in annealed condition +A

  • Tensile strength, Rm: 450 - 650 MPa
  • The yield point, Re: > 250 MPa
  • Elongation, A:> 18%
  • Hardness, HB: <200
  • Module of elasticity, E: 220 GPa
  • Linear expansion coefficient, α20℃: 10,4 * 10-6 K-1
  • Thermal capacity, cp = 430 J * kg-1 * K-1
  • Thermal conductivity, λ = 25 W * m-1 * K-1
  • Specific resistance, Ω: 0,6 mkOhm * m

 


Mechanical properties at elevated temperatures

Properties Temperature
100℃ 200℃ 300℃ 400℃ 500℃
Linear expansion coefficient, α (*10-6 K-1) 10,4 10,8 11,2 11,6 11,9
The yield point, Rp0,2 (MPa) >240 >220 >210 - -
Modulus of elasticity, E (GPa) 215 210 205 195 -

 


Heat treatment - processes and temperature

  • Rolling and forging at 1100 - 800℃ with cooling in the air
  • Annealing + A at 680 - 760℃ with cooling in water or air

 

In the aforementioned grades we supply companies with:

 


Other grades designations:

X2CrNi12, X 2 CrNi 12, 1.4003, AISI 410L, SUS 410L, UNS S40977, 3Cr12, S41003, 022Cr12Ni, Z8CNT12, Z 8 CNT 12.


THIS WEBSITE USES COOKIES TO IMPROVE AND FACILITATE YOUR ACCESS TO THE WEBSITE AND TO KEEP STATISTICS. IF YOU CONTINUE TO USE THIS SITE, YOU AGREE THAT THE COOKIES WILL BE STORED ON YOUR DEVICE
PRIVACY POLICY
How do I disable cookies
AGREE